High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 16".Information provided by Anderman Ceramics.
Physical Properties Metric English Comments
Density 3.92 g/cc
0.142 lb/in³
Open Porosity 0.00 %
0.00 %
Gas Tight
Mechanical Properties Metric English Comments
Hardness, Mohs 9.0
9.0
Tensile Strength 172 MPa
25000 psi
Flexural Strength 320 MPa
46400 psi
Thermal Properties Metric English Comments
CTE, linear 8.60 µm/m-°C
4.78 µin/in-°F
8.00 µm/m-°C

@Temperature 20.0 - 1000 °C
4.44 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 27.0 W/m-K

@Temperature 20.0 - 100 °C
187 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1750 °C
3180 °F
Component Elements Properties Metric English Comments
Al2O3 99.8 %
99.8 %
B2O3 <= 0.020 %
<= 0.020 %
CaO 0.030 %
0.030 %
Fe2O3 0.020 %
0.020 %
MgO 0.030 %
0.030 %
Na2O 0.15 %
0.15 %
SiO2 0.050 %
0.050 %
TiO2 <= 0.010 %
<= 0.010 %
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
1.00e+8 ohm-cm

@Temperature 600 °C
1.00e+8 ohm-cm

@Temperature 1110 °F
Dielectric Constant 9.8

@Frequency 1.00e+6 Hz
9.8

@Frequency 1.00e+6 Hz
Descriptive Properties Value Comments
Thermal Shock Resistance Good