Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 173 MPa | 25000 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BFG30-AS00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 172 MPa | 25000 psi | |
Anderman Ceramics EA995 Sintered Alumina, 99.5% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Tensile Strength | 172 MPa | 25000 psi | |
Anderman Ceramics EA998 Sintered Alumina, 99.8% High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 1.. |