Material Notes:
Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Carbon/Glass Fibers, Advanced Composite Structures, Ribs and Flat Surfaces, High ModulusInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 116
116
ASTM D785
Tensile Strength, Ultimate 517 MPa
75000 psi
ASTM D638
Tensile Modulus 86.2 GPa
12500 ksi
ASTM D638
Flexural Strength 662 MPa
96000 psi
ASTM D790
Flexural Modulus 55.2 GPa
8000 ksi
Tangent; ASTM D790
Compressive Strength 206 MPa
29900 psi
ASTM D695
Izod Impact, Notched 10.7 J/cm
20.0 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.030
0.030
% Loss 1000 Cycles; FTMS1091
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
Flexural Load; ASTM D648