Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.68 g/cc | 0.0607 lb/in³ | |
Parker Chomerics CHO-SHIELD® 4914 Conductive Coating Conductive Solvent-Resistant Acrylic Coating. Formulated for high resistance to solvent attack, CHO-SHIELD® 4914 is an electrically conductive, one-component acrylic coating. Compared to zinc arc s.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded
&nbs AMODEL AFA-6133 V0 is a 33% glass-fiber reinforced grade of polyphthalamide (PPA) resin that was developed specifically for connector applications requiring compatibility with both "infrared" and "v.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Density | 1.68 g/cc | 0.0608 lb/in³ | |
Garlock 2900 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation .. |
|||
Density | 1.68 g/cc | 0.0608 lb/in³ | |
Garlock 2930 Compressed Aramid Fiber Gasketing, Neoprene Binder Aramid fibers with a Neoprene binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, steam, refrigerants, oils, fuels, mild acids, and.. |
|||
Density | 1.68 g/cc | 0.0608 lb/in³ | |
Garlock 9850 Compressed Carbon Fiber Gasketing, Nitrile Binder Carbon fibers with a nitrile binder.Carbon fiber gasketing excels in harshest conditions - intense heat, high pressure, saturated steam and hot oils.Laboratory-tested for fire safety.Long-lasting se.. |
|||
Density | 1.68 g/cc | 0.0608 lb/in³ | |
Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder Carbon fibers with a SBR binder.Carbon fiber gasketing excels in harshest conditions- intense heat, high pressure, saturated steam and hot oilsLaboratory tested for fire safetyMaintains effective se.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 216 L2 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, UV stabilized and characterized by a high fluidity of the melt, for injection molding.Available in: Europe and North America Pr.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D1505 |
Solvay Specialty Polymers Halar® 6514 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® 6514 is a black, semi-crystalline melt processable fluorinated primer. It is designed to be applied directly to substrates by electrostatic or fluidized bed techniques. In particular Halar.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Density | 1.68 g/cc @Temperature 25.0 °C |
0.0607 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® SV80 PFPE Solvent Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D792 |
Techmer ES HiFill® PPA GF45 HS L X 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat Stabilizer, Mold Release and LubricantFeatures: Heat Stabilized, Gold Mol.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | |
UCAR Carbon UCAR® ATR Isostatic Molded Graphite Isostatically molded ATR is a lower density version of grade ATJ. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish.Typical Application.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | Relative Density; ISO 1183 |
Vyncolit X680 Novolac Phenolic Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with t.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | DIN 53479 |
Polyram RamSter PF320G6 PBT, 30% Glass Fiber, Flame Retardant 30% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183 |
Polyplastics Duranex® 353RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | dry; ISO 1183 |
DSM Stanyl® 46SF5030 PA46-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Density | 1.68 g/cc | 0.0606 lb/in³ | |
Devcon Brushable Ceramic - Red, Blue Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183 |
Barlog Plastics KEBATER A9045 PBT, 45% glass fiber reinforced, improved surface quality, reduced warpage, food grade (PBT+X)-GF45Information provided by BARLOG plastics GmbH. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183 |
BASF Petra® 130 FR BK-112 30% Glass Filled PET Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183 |
BASF Ultradur B 4406 G6 Q717 30% Glass Filled PBT Ultradur B 4406 G6 Q717 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D3275 |
Solvay Specialty Polymers Halar® 6514 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)&l Halar 6514 is a black, semi-crystalline melt processable fluorinated primer. It is designed to be applied directly to substrates by electrostatic or fluidized bed techniques. In particular Halar 651.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D792 |
Westlake Plastics Halar® 901 ECTFE Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impa.. |
|||
Density | 1.68 g/cc | 0.0607 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Density | 1.68 - 1.88 g/cc | 0.0607 - 0.0679 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |