Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Applied Nanostructured Solutions Carbon NanoStructure Encapsulated Flakes

Category Carbon , Carbon Fiber , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Carbon Fiber Filled
Manufacturer Applied Nanostructured Solutions
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Nanostructured Solutions Carbon NanoStructure Encapsulated Flakes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon NanoStructure (CNS) Encapsulated Flakes are a unique form of carbon nanotubes, produced using a proprietary ANS process. The ANS process creates cross-linked multiwall carbon nanotube-based net-works of CNS with a distinctive morphology that, when added to polymers, elastomers and thermoplastics, enhance the resulting products with multifunctional properties, such as increased conductivity and dramatically improved strength and modulus. These properties allow for the replacement of metal parts with CNS-infused thermoplastics containing a very small amount of CNS, which result in significant cost savings.*Properties are for PC/ABS w/ added 3% CNS by weightInformation provided by Applied Nanostructured Solutions (ANS)
Physical Properties Metric English Comments
Bulk Density 0.135 g/cc
0.00488 lb/in³
Thickness 10.0 microns
0.394 mil
Mechanical Properties Metric English Comments
Tensile Strength 87.0 MPa
12600 psi
Tensile Modulus 4.61 GPa
669 ksi
Flexural Strength 125 MPa
18100 psi
Flexural Modulus 3.51 GPa
509 ksi
Component Elements Properties Metric English Comments
Loss on Ignition(%) >= 93 %
>= 93 %
Electrical Properties Metric English Comments
Shielding Effectiveness 40 dB

@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
40 dB

@Thickness 0.118 in,
Frequency 3.00e+7 Hz
3% CNS; ASTM D4935
50 dB

@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
50 dB

@Thickness 0.118 in,
Frequency 2.03e+9 Hz
3% CNS; ASTM D4935
51 dB

@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
51 dB

@Thickness 0.118 in,
Frequency 3.00e+7 Hz
5% CNS; ASTM D4935
60 dB

@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
60 dB

@Thickness 0.118 in,
Frequency 2.03e+9 Hz
5% CNS; ASTM D4935
Processing Properties Metric English Comments
Moisture Content <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
% Sizing, type ~4%
Polyurethane, Polyimide, Polyamide
Chop Length 70µm