Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.135 g/cc | 0.00488 lb/in³ | |
Applied Nanostructured Solutions Carbon NanoStructure Encapsulated Flakes Carbon NanoStructure (CNS) Encapsulated Flakes are a unique form of carbon nanotubes, produced using a proprietary ANS process. The ANS process creates cross-linked multiwall carbon nanotube-based n.. |