Arkema Group Appryl® 3130 MU 7 Polypropylene - Polyethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Arkema
Trade Name Appryl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Appryl® 3130 MU 7 Polypropylene - Polyethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP/PE copolymer colored during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive industry. It is UV stabilized.ISO data provided by the manufacturer, Arkema.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.5 MPa
3120 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 8.0 %
8.0 %
50 mm/min
Tensile Modulus 1.03 GPa
149 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
Vicat Softening Point 60.0 °C
140 °F
50°C/hr; 50N