Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group KYNAR® Latex 32 Polyvinylidene Fluoride

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Arkema
Trade Name KYNAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group KYNAR® Latex 32 Polyvinylidene Fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Water base, fine particle sizeInformation provided by Arkema Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Density of solids
Density 2.23 g/cc
0.0805 lb/in³
Solids Content 18 %
18 %
Thermal Properties Metric English Comments
Melting Point 155 - 160 °C
311 - 320 °F
Users viewing this material also viewed the following: