Thermal Properties Metric English Comments
Melting Point 155 °C
311 °F
Flow temperature, ASTM D569-59
Rotuba 860H2 Ethyl Cellulose
Data provided by the manufacturer.
Melting Point 155 °C
311 °F
Flow temperature, ASTM D569
Rotuba H Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Melting Point 155 - 170 °C
311 - 338 °F
ASTM D3418
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer
NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co..
Melting Point 155 - 165 °C
311 - 329 °F
MQSA 111
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1..
Melting Point 155 - 160 °C
311 - 320 °F
Hong Kun Group AO 1098 Antioxidant
Chemical Name: 3,3'-Bis(3,5-di-tert-butyl-4-hydroxyphenyl)-N,N'-hexamethylenedipropionamideCAS No. 23128-74-7All information provided by Hongkun Group
Melting Point 155 - 173 °C
311 - 343 °F
Huntsman/TMA
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop..
Melting Point >= 155 °C
>= 311 °F
ISO 3146-C
FKuR Kunststoff Bio-Flex® F 1130 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Melting Point 155 °C
311 °F
Peak
LG Chemical KEYFLEX BT 10288D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Melting Point 155 °C
311 °F
DIN EN ISO 314
GEHR Plastics PA 12 TR Transparent Nylon 12
Used for optical components that benefit from the transparency and the high dynamic strengthProperties:TransparencyExtremely high dynamic strengthHigh chemical resistanceHigh stress-cracking resista..
Melting Point 155 °C
311 °F
TMA; MCI Method
Mitsui APELâ„¢ APL6015T Cyclo Olefin Copolymer (COC)
This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces..
Melting Point 155 - 165 °C
311 - 329 °F
MQSA 111
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ..
Melting Point 155 °C
311 °F
ASTM D2117
Lushan PR296B Adhesive Resin for Aluminum Plastic Composite Pipe
Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides i..
Melting Point 155 - 175 °C
311 - 347 °F
Huntsman/TMA
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether
Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext..
Melting Point 155 °C
311 °F
ASTM D3418
SK Chemicals SKYPEL G140D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Melting Point 155 °C
311 °F
Kofler
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane
Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf..
Melting Point 155 - 159 °C
311 - 318 °F
ISO 3146
Borealis Daploy™ SF203HMS High Melt Strength Polypropylene for Extrusion Coating
Daploy SF203HMS resin is a statistic-heterophasic-propylene-ethylene copolymer modified with a polypropylene based structurally isomeric polymer which combines a significantly increased melt strengt..
Melting Point 155 °C
311 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® 30HS Polyester Elastomer TPC-ET  (Unverified Data**)
Polyester Elastomer Concentrate Developed for Enhancing Heat Ageing ResistanceInformation provided by DuPont Performance Polymers
Melting Point 155 °C
311 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® 4053FG TPC-ET  (Unverified Data**)
Hytrel® 4053FG is a low modulus high performance thermoplastic elastomer with food compliance specificity. It is suitable for extrusion and injection molding processes.Information provided by DuPon..
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Melting Point 155 - 165 °C
311 - 329 °F
Arkema Group KYNAR® 461 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Melting Point 155 °C
311 °F
ISO 3146
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Melting Point 155 - 165 °C
311 - 329 °F
Arkema Group KYNAR® 301-F Polyvinylidene Fluoride Powder
Characteristics: Fine milled, white, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abra..
Melting Point 155 - 165 °C
311 - 329 °F
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Melting Point 155 - 165 °C
311 - 329 °F
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR® Latex 32 Polyvinylidene Fluoride
Water base, fine particle sizeInformation provided by Arkema Inc.
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850 PC Polyvinylidene Fluoride Spray Coating Powder
Electrostatic sprayInformation provided by Arkema Inc.
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Melting Point 155 - 165 °C
311 - 329 °F
Arkema Group KYNAR® 201 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..