Material Notes:
Polyether block amide PEBAX® MV 1074 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 1074 SP 01 is an inherently dissipative polymer and can be dry blended or compounded with an isolative polymer to lower the surface resistivity. This SP grade has been developed to be heat and UV resistant.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Water Absorption 48 %

@Temperature 23.0 °C,
Time 86400 sec
48 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.4 %

@Temperature 20.0 °C
1.4 %

@Temperature 68.0 °F
50% RH; ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
Instantaneous, Conditioned 15 days at 23°C - 50% RH; ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Elongation at Break >= 700 %
>= 700 %
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Flexural Modulus 0.0800 GPa
11.6 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Thermal Properties Metric English Comments
Melting Point 158 °C
316 °F
ISO 11357
Optical Properties Metric English Comments
Refractive Index 1.502
1.502
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+9 ohm-cm
2.50e+9 ohm-cm
IEC 60093
Surface Resistivity per Square 3.00e+9 ohm
3.00e+9 ohm
IEC 60093
Static Decay <= 1.0 sec
<= 1.0 sec
MIL B-81705