Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties even at low temperatures. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Good dimensional stability (low moisture absorption).Example applications: Flexible parts with high impact strength and vibration resistance.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 1.2 %
1.2 %
Melt Flow 48.8 g/10 min

@Load 2.16 kg,
Temperature 235 °C
48.8 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 26 %
26 %
50 mm/min
Tensile Modulus 0.440 GPa
63.8 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 168 °C
334 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Electrical Properties Metric English Comments
Dissipation Factor 0.00036

@Frequency 1e+6 Hz
0.00036

@Frequency 1e+6 Hz
0.00123

@Frequency 100 Hz
0.00123

@Frequency 100 Hz
Users viewing this material also viewed the following: