Material Notes:
Powder T BLUE X 7421 AC - RILSAN POLYAMIDE 11 (PA11) POWDERBlue Powder pigmented by Dry Blend, designed for the coating of tubes, pipe systems, flanges and fittings for the transport of fluids in particular potable water.Coating done by dipping of pre heated part in a bed of fluidized powder.Submitted to potable water approval.The range includes several colors.The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Water Absorption 1.9 %
1.9 %
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
10°C/min
Vicat Softening Point 160 °C
320 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 30.0 kV/mm
762 kV/in