Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Radici Radilon® CA RV300L (cond.) Nylon 66/6 Radilon® CA is a range of polyamide 66/6 copolymers obtained through the polymerization of hexamethylendiamine, adipic acid and caprolactam.Information provided by Radici group. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Radici Radilon® S 35HR (cond.) Nylon 6 PA6 medium-high viscosity injection molding grade. Easy mould release.Information provided by Radici group. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Radici Radilon® S RV500 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Polimeri Europa SINKRAL B260 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-04-09-25 Very high heat injection moulding grade with good impact resistance for this category of ABS. Main.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Polimeri Europa SINKRAL PD H210/K ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,085-25-16-25 Flame retarded (PBBE free) injection moulding grade, rated UL94-5V at 3.2 mm thick and UL 94V-0 at.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
Celanese Hostaform® C 9021 GV1/30 POM, 30% Glass Reinforced
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 26 % glass fibersInformation provided by Celanese |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
DSM Akulon® K224-G3U (Cond.) 15% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
LyondellBasell Lupolen® 6021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small, rigid, thin-walled containers (up to 5 l), pots (up to 1 l), bottles and canisters (up to 5 l) for packaging mineral oil, antifreeze, brake fluid; drink bott.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
LyondellBasell Lupolen® 1810 D LDPE Blow moldings, sheet, profile, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Surface Resistance | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ASTM D257 |
Solvay Specialty Polymers Ajedium™ PVDF 9009 Polyvinylidene Fluoride (PVDF) Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea.. |
|||
Surface Resistance | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ASTM D257 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Surface Resistance | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ASTM D257 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Surface Resistance | >= 1.00e+14 ohm | >= 1.00e+14 ohm | IEC 93 |
Supreme Petrochem SP 555 Flame Retardant Polystyrene Characteristics Very good flow properties Good balance of toughness and rigidity Available in any dark colors Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxe.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257, IEC 93 |
EPICHEM Epiter PBT GF 20 Polybutylene Terephthalate, 20% Glass Characteristics: 20% glass fibre filled |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, heat stabilized, black Information provided by Eurotec® |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257, IEC 93 |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS Characteristics: Thermic resistant |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
Eurotec® Tecodur® PB70 KK45 NL XA 20 PBT 45% glass fiber/mineral reinforced, UL94 V0, low warpage Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to .. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Arkema Group Rilsan® Powder D40 Natural Nylon 11, Coating Grade Powder D40 NATURAL - RILSAN POLYAMIDE 11 (PA11) POWDERUnpigmented and clear Powder as an additive for paints. Improves the scratch and abrasion resistance of paints. Allows for different texture d.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
BASF Polystyrol® 143 E Polystyrene (Europe) Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | CEI 60093 |
Addiplast Addilene PMD 50284 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | Conditioned; CEI 60093 |
Addiplast Addinyl A2 Nylon 66 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend Flame retardant grade with very high heat resistance; used for precision parts and where the material must withstand high injection temperatures (e.g. heater-fan impellers).Data was collected by ISO.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
DSM Akulon® K-FG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Polimeri Europa SINKRAL D720 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-08-35-15 High impact injection moulding grade, with improved flow compared with SINKRAL B620 and a high glo.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Arkema Group Oroglas® MI-7T Acrylic
(discontinued **) OROGLAS MI-7T is a medium impact grade combining excellent thermal resistance with good impact performance.Key features : impact resistance: up to 7 times more impact-resistant than standard acr.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
Techmer ES HiFill FR® PBT GF30 FR-S 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Non-BloomingProcessing Method: Injection MoldingInformation provided by .. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
DSM Akulon® K-FKGS6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |