Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 48362X005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 48362X005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassProduct Use: Flexible hose/duct substrateAppearance: Gray silicone rubber on fiberglass fabricThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 50.8 microns
2.00 mil
Side 1; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Substrate; Arlon SQA-TMS-003
127 microns
5.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
Silicone Property; ASTM D2240
Tensile Strength 6.89 MPa
1000 psi
Silicone Property; ASTM D412
Elongation at Break 275 %
275 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability Test 0.00
0.00
[sec], After Flame Time
0.50
0.50
[in], Flame Propagation
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
Total Product Weight (oz/yd2) 5.6
Arlon SQA-TMS-025