Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 10502R020 0.020" (0.508 mm) Cured Silicone Rubber (Unsupported) Design/Construction:Material: Cured Silicone RubberLiner: Polyethylene Recommended Cure Cycle: Product delivered curedRecommended Post Cure Cycle: Product delivered post-curedAppearance: Red silicon.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 10842R125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 32980X040 0.040" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51044R020 0.020" Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Semi-cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should no.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51366X015 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Flame Resistance: Product is designed to meet Title 14 CFR.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51579XA028 0.028" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material a.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51599R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55572XD028 0.028" (0.711 mm) Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55580R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values for th.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55589W028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55989R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R35928R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R36319R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 30580R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 30850S125 0.125" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 44571XB015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate) Side 2: Uncured Silicone RubberInterleave: 2.5 mil .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 44576R016 0.016" (0.406 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 47576R007 0.0075" (0.190 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mate.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 49283R040 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil polyethylene; Side 1: cured silicone rubber; Substrate: 1681 Fiberglass; Side 2: cured silicone rubber |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51576W015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: White silicone gum on glass fabricThis data re.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 51581R018 0.018" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R30342R032 0.032" (0.813 mm) Cured Silicone Rubber Design/Construction:Product: Cured Silicone Rubber Liner: PolyethyleneAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to w.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon R34260N005 0.005" (0.127 mm) Unsupported/Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured Rubber Appearance: Clear gum on release linersThis data Represents typical values for the production material. The data should not be used to write, o.. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 45561R007 0.007"(0.178 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not .. |
|||
Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
Arlon 44406X015 0.015" (0.381 mm) Platinum Cured Silicone/Peroxide Catalyzed Silicone Design/Construction:Side 1: Platinum Cured SiliconeSide 2: Peroxide Catalyzed SiliconeAppearance: Gray silicone gum on fiberglass clothThis data represents typical values for the production material.. |