Arlon LW301Bxx-P0 0.030" Self-Fusing Silicone Rubber Tape

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon LW301Bxx-P0 0.030" Self-Fusing Silicone Rubber Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1 inch wide, 30 mil thick, black, triangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Design/Construction:Rubber: Cured Self-fusing Silicone RubberCross-section: 1" wide triangularInterleave: 2.5 mil PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 762 microns
30.0 mil
Rubber; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 9.467 MPa
1373 psi
Silicone Property; Arlon SQA-TMS-009
Elongation at Break 481 %
481 %
Silicone Property; Arlon SQA-TMS-009
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Allis Chalmers Tack (inches) 0.25
Arlon SQA-TMS-013
Color Black
Tape
White
Guideline