Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 9.467 MPa
1373 psi
Silicone Property; Arlon SQA-TMS-009
Arlon LW301Bxx-P0 0.030" Self-Fusing Silicone Rubber Tape
1 inch wide, 30 mil thick, black, triangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Des..
Tensile Strength 9.467 MPa
1373 psi
Silicone Property; Arlon SQA-TMS-009
Arlon LW40125B12-P0 0.040" Self-Fusing Silicone Rubber Tape
1.25 inches wide, 40 mil thick, black, triangular cross-section, self-fusing silicone tape. Product is supplied in 12 yard long roll lengths.Design/Construction:Rubber: Cured Self-fusing Silicone R..