Material Notes:
Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15 ); 0.003 in. (0.8 mm) polyethylene interleave. Color: Translucent. Weight: 2339 g/m² ± 234 (69.0 oz./yd.² ± 6.9).Applications: Composite vacuum bagging materials.Information provided by the manufacturer, Arlon Silicone Technologies Division.
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
Tensile Strength, Ultimate 7.47 - 9.13 MPa
1080 - 1320 psi
Elongation at Break 540 - 660 %
540 - 660 %
100% Modulus 0.00172 GPa
0.249 ksi
Average
Tear Strength >= 43.8 kN/m
>= 250 pli
Compression Set 28 %
28 %
after post cure
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.6 °C
-69.9 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.75 kV/mm
>= 400.0 kV/in