Material Notes:
Fluon®LM-ETFE combines the excellent properties in heat resistance and other mechanical properties owned by ETFE resin and the low melting point.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.78 g/cc
1.78 g/cc
ASTM D792
Melt Flow 20 - 30 g/10 min
20 - 30 g/10 min
ASTM D359
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 0.647 GPa
93.8 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
Flammability, UL94 V-0
V-0
Oxygen Index 40 %
40 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 2.4

@Frequency 1000 Hz
2.4

@Frequency 1000 Hz
ASTM D150
2.4

@Frequency 1e+6 Hz
2.4

@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.00070

@Frequency 1000 Hz
0.00070

@Frequency 1000 Hz
ASTM D150
0.0082

@Frequency 1e+6 Hz
0.0082

@Frequency 1e+6 Hz
ASTM D150
Descriptive Properties Value Comments
10% Weight Loss °C 410
Anti cracking at 200°C excellent
Heat Ageing (retention of elongation) 120%
Heat Ageing (retention of tensile strength) 88%