Mechanical Properties Metric English Comments
Flexural Modulus 0.647 - 1.37 GPa
93.8 - 199 ksi
Average value: 1.06 GPa Grade Count:15
Overview of materials for Modified ETFE, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap..
Flexural Modulus 0.647 - 0.686 GPa
93.8 - 99.5 ksi
ASTM D790
Daikin NEOFLON AP-210AS PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D..
Flexural Modulus 0.647 - 0.686 GPa
93.8 - 99.5 ksi
ASTM D790
Daikin NEOFLON AP-230ASL PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc...
Flexural Modulus 0.647 - 0.686 GPa
93.8 - 99.5 ksi
ASTM D790
Daikin NEOFLON AP-201 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil..
Flexural Modulus 0.647 - 0.686 GPa
93.8 - 99.5 ksi
ASTM D790
Daikin NEOFLON AP-210 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided ..
Flexural Modulus 0.647 - 0.686 GPa
93.8 - 99.5 ksi
ASTM D790
Daikin NEOFLON AP-230 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries.
Flexural Modulus 0.647 GPa
93.8 ksi
ASTM D790
Asahi Glass Fluon® LM-730AP LM-ETFE Fluororesin
Fluon®LM-ETFE combines the excellent properties in heat resistance and other mechanical properties owned by ETFE resin and the low melting point.Information provided by Asahi Glass Company, Inc.