Asahi Kasei Thermofil P-40TC-1156 40% Talc Reinforced, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil P-40TC-1156 40% Talc Reinforced, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 29.6 MPa
4300 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Strength 49.6 MPa
7200 psi
ASTM D790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.14 J/cm
4.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648