Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 261WO PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 261WO PPO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose V-0 rated resin with good impact strength.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ATSM D638
Elongation at Yield 40 %
40 %
ASTM D638
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Flammability, UL94 V-0
V-0