Ashley Polymers Ashlene® 559LD-33G Nylon 66, 33% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 559LD-33G Nylon 66, 33% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high impact reinforced nylon copolymer with good low temperature properties.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 145 MPa
21000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Modulus 7.00 GPa
1020 ksi
ASTM D790
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 231 °C
448 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 229 °C
444 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 218 °C
424 °F
ASTM D648