Ashley Polymers Ashlene® 734LD Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 734LD Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A plasticized, highly flexible Nylon 6 with high impact resistance.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hrs; ASTM D570
Moisture Absorption at Equilibrium 2.2 %
2.2 %
ASTM D570
Water Absorption at Saturation 7.7 %
7.7 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ATSM D638
Elongation at Break 315 %
315 %
ASTM D638
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
Izod Impact, Notched 5.33 J/cm
9.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648