Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent flexural, impact, and tensile characteristics Very high continuous working temp Very high heat distortion temp Exceptional chemical resistance Superior dielectric at high temperatures and frequencies Good radiation resistance Outstanding wear and abrasion resistance Low smoke and toxic gas emissions Excellent hydrolysis resistance Information provided by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Water Absorption 0.11 %
0.11 %
at 24 hours; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 103
103
ASTM D785
Tensile Strength, Yield 157 MPa
22800 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Tensile Modulus 9.6995 GPa
1406.8 ksi
1 % Sec; ASTM D638
Flexural Strength 233 MPa
33800 psi
ASTM D790
Flexural Modulus 10.309 GPa
1495.2 ksi
Tangent; ASTM D790
Compressive Strength 215 MPa
31200 psi
ASTM D695
Shear Strength 97.2 MPa
14100 psi
Ultimate; ASTM D3846
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 21.6 µm/m-°C

@Temperature 20.0 °C
12.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.432 W/m-K
3.00 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 334 °C
633 °F
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 316 °C
600 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Surface Resistivity per Square 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Strength 6.89 kV/mm
175 kV/in
ASTM D149
Users viewing this material also viewed the following: