Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 30% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 30% glass reinforced heat and light stabilized Nylon 12.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 97.0 MPa
14100 psi
ATSM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Modulus 6.80 GPa
986 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 184 °C
363 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 177 °C
351 °F
ASTM D648