Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 184 - 263 °C
363 - 505 °F
Indium Corp. Indalloy 144 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Melting Point 184 - 270 °C
363 - 518 °F
Indium Corp. Indalloy 146 Lead Solder Alloy
Information Provided by Indium Corporation
Melting Point 184 - 210 °C
363 - 410 °F
Indium Corp. Indalloy® 7 In-Pb Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
Melting Point 184 - 209 °C
363 - 408 °F
Williams Advanced Alloys WS209 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 184 °C
363 °F
Crystalline melt point; Hot stage
Arlon CuClad 6700 Bonding Film
Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu..
Melting Point 184 °C
363 °F
ASTM D3418
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer
This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire..
Melting Point 184 °C
363 °F
ASTM D3418
Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced
A 30% glass reinforced heat and light stabilized Nylon 12.Data provided by the manufacturer
Melting Point 184 °C
363 °F
ASTM D3418
Ashley Polymers Ashlene® D926 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl..
Melting Point 184 °C
363 °F
ASTM D3418
Ashley Polymers Ashlene® D927 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl..
Melting Point 184 °C
363 °F
ASTM D3418
Ashley Polymers Ashlene® D930H Nylon 12
A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. Also UV and heat stabilized, available in natural and precolored. Any color other than natural ..
Melting Point 184 °C
363 °F
ASTM D3418
Ashley Polymers Ashlene® L927 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability, and low moisture absorption. Also availab..
Melting Point 184 °C
363 °F
ASTM D3418
Ashley Polymers Ashlene® L930 Nylon 12
A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. The natural color is slightly darker.Data provided by the manufacturer
Melting Point 184 °C
363 °F
ASTM D3418
Ashley Polymers Ashlene® D925 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl..
Melting Point 184 °C
363 °F
ASTM D3418
Ashley Polymers Ashlene® L925 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. The natural c..
Melting Point 184 °C
363 °F
ASTM D3418
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer
Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized..
Melting Point 184 °C
363 °F
ASTM D3418
ALM PA 620-MF Mineral Fiber Filled Nylon 12 SLS Prototyping Polymer
Information provided by Advanced Laser Materials (ALM).