Ashley Polymers Ashlene® P1043R Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, UV Stabilized
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® P1043R Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose, injection molding grade, natural resin containing UV stabilizer.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Moisture Absorption at Equilibrium 0.34 %
0.34 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
Cond. O
Mechanical Properties Metric English Comments
Hardness, Rockwell M 71
71
ASTM D785
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 7.74 J/cm
14.5 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
264 °F
ASTM D648