Ashley Polymers Ashlene® RH180 Acetal

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® RH180 Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion grade reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. Available in Natural and Black. Natural is designated RH180; Black is designated RH180B.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.022 cm/cm
0.022 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Melt Flow 2.5 - 3.0 g/10 min
2.5 - 3.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.0 MPa
9140 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
ASTM D3418