Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 175 °C | 347 °F | ISO 11357-1 |
Murtfeldt Murinyl® Polyvinylidinefluoride As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur.. |
|||
Melting Point | 175 °C | 347 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet) |
|||
Melting Point | 175 °C | 347 °F | DSC, both heating and cooling speeds of 10°C/min |
Noltex Soarnol® BG3522 Ethylene Vinyl Alcohol Copolymer Special designed high MFI grade. New EVOH for extrusion coating. Ethylene content 35 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, .. |
|||
Melting Point | 175 °C | 347 °F | Flow temperature, ASTM D569 |
Rotuba H5 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Melting Point | 175 °C | 347 °F | DSC |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Melting Point | 175 - 178 °C | 347 - 352 °F | Average value: 177 °C Grade Count:5 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melting Point | 175 - 188 °C | 347 - 370 °F | Huntsman/TMA |
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melting Point | 175 °C | 347 °F | DIN 53736 |
Isoflon POM H Polyacetal H Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Melting Point | 175 - 187 °C | 347 - 369 °F | Huntsman/TMA |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
Melting Point | 175 °C | 347 °F | DSC |
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
Melting Point | 175 °C | 347 °F | ISO 11357 |
Polyram PlusTek PD120BK11 Nylon 12 for Extrusion, UV Stabilized Nylon 12 UV stabilized for extrusion application.Information provided by Polyram. |
|||
Melting Point | 175 °C | 347 °F | ISO 11357 |
Polyram PlusTek PD300G5 Nylon 12 for Injection Molding, 25% Glass-Fiber Reinforced 25% Glass-fiber reinforced Nylon 12, heat stabilized and hydrolysis resistant for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 175 °C | 347 °F | |
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber 30% glass fiber reinforced, high thermal resistance high UV and radiation PVDF for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | <= 175 °C | <= 347 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 7521 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7521 is a high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesiv.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D2133 |
Ensinger Delrin® 150 Homopolymer Acetal (POM) Ensinger's Delrin® 150 stock shapes are a homopolymer acetal manufactured using DuPont Delrin 150 Resin. It is a crystalline plastic which offers an excellent balance of properties to bridge the g.. |
|||
Melting Point | 175 °C | 347 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ensinger DELRIN® 507 Black Acetal Homopolymer (POM) Delrin® 507 is a general purpose homopolymer acetal containing a UV stabilizer ideally suited for outdoor applications or those in which there is an otherwise abundant source of UV light.General hi.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM) DELRIN®570 Shapes manufactured by Ensinger are 20% glass filled materials intended for general industrial use. The material offers very high stiffness, low warpage, and low creep for superior part .. |
|||
Melting Point | 175 °C | 347 °F | |
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM) Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an excep.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ashley Polymers Ashlene® RH190-PF Acetal, PTFE Filled A wear-resistant grade homopolymer resin with 1.5% PTFE.Data provided by the manufacturer |
|||
Melting Point | 175 - 195 °C | 347 - 383 °F | DSC Induction Temperature; TM-029 |
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Melting Point | 175 - 195 °C | 347 - 383 °F | DSC Induction Temperature; TM-029 |
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ashley Polymers Ashlene® RH190H Acetal General purpose reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated RH190H-.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3417 |
Quantum Acetal-Homopolymer Information provided by Quantum Advanced Engineering Plastics |