Axiall 02520 Plenum Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 02520 Plenum Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-lead stabilized plenum grade jacket with good low temperature properties. Recommended for Category 5 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.54 - 1.58 g/cc
1.54 - 1.58 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 48 - 54
48 - 54
delayed; ASTM D-2240
Tensile Strength, Yield 15.9 MPa
2300 psi
ASTM D-638
Elongation at Yield 225.3 %
225.3 %
Air Aging: 10 days @ 100°C; 30 mil slabs; UL 1581
250 %
250 %
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -16.0 °C
3.20 °F
ASTM D-746
Oxygen Index 43 %
43 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F