Material Notes:
Battery booster jacket compound and general purpose jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 83 - 89
83 - 89
delayed; ASTM D-2240
Tensile Strength, Yield 15.2 MPa
2200 psi
ASTM D-638
Elongation at Yield 350 %
350 %
ASTM D-638
100% Modulus 0.00793 GPa
1.15 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D-746
Oxygen Index 23.5 %
23.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F