Material Notes:
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.22 - 1.26 g/cc
1.22 - 1.26 g/cc
ASTM D-792
Melt Flow 47.71 g/10 min

@Load 23.9 kg,
Temperature 175 °C
47.71 g/10 min

@Load 52.7 lb,
Temperature 347 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
delayed; ASTM D-2240
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D-638
Elongation at Yield 375 %
375 %
ASTM D-638
100% Modulus 0.00965 GPa
1.40 ksi
ASTM D-638
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F
Users viewing this material also viewed the following: