Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D412 |
S&E Specialty Polymers GA-1050-OR3-LF PVC Application: Lead free, 105° C PVC insulating compound designed for SJEOO applications. Complies with RoHS requirements.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D412 |
S&E Specialty Polymers GA-1941-AFRO PVC Application: 105° C PVC insulating compound designed for SJEOO applicationsInformation provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S190A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D412 |
Lubrizol Estane® 2355-95AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Fuel resistant, extrusion laminate coatingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Dow Chemical.Lubrizol acquired the Pellethane.. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 835WA Wire & Cable Flexible PVC AWM for SPT, SJT and SVT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 8820 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound designed for use in weatherstrips, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall EX 3154 Plenum Flexible PVC Non-lead stabilized CAT 3 plenum jacket. Recommended for up to 25 pair, unshielded.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D412 |
ACC SMP™ EP 3001 EPI Engineered Polymers Silicone Modified Polymer EP 3001, “Powered by Reactamine® Technology”, is a two component 100% solid polyurea based sealant. EP 3001 is a self-leveling sealant designed to protect horizontal concrete. This elastomer disp.. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 10870 Wire & Cable Flexible PVC General purpose jacket compound recommended for 60C applications and also suited for 75C at a wall thickness of 30 mils and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 11850 Wire & Cable Flexible PVC General purpose fungus and microbe resistant clear PVC compound. Also formulated for good UV resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 13840 Coax & Telecom Flexible PVC Economical CATV coaxial cable jacket. Also suitable for CL2 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 1801 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 190 Moldings & Extrusions Flexible PVC 60C plug molding component. UL recognized component for 94 V-0 in all colors. 1.13 mm minimum thickness. UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axia.. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 312 Wire & Cable Flexible PVC General purpose jacketing and insulation compound. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 8823 Moldings & Extrusions Flexible PVC A UL certified flame retardant, clear flexible PVC compound recommended for a maximum service temperature of 60°C. Exhibits good migration resistance properties. UL approved for 94 V-0 at 2.30 mm.. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | ASTM D-638 |
Axiall 8830 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, shapes, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00965 GPa | 1.40 ksi | 1:1; ASTM D412 |
ACC EP JS EPI Engineered Polymers Joint Sealant EP JS Joint Sealant JS, “Powered by Reactamine® Technology” is a two component 100% solid (silicone optional) polyurea based joint sealant. EP JS is a self-leveling joint sealant designed to prot.. |