Axiall 22951 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 22951 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-lead stabilized, 75C rated jacket compound suitable for riser constructions over HDPE.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.46 - 1.50 g/cc
1.46 - 1.50 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 92 - 98
92 - 98
delayed; ASTM D-2240
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D-638
Elongation at Yield 240.6 %
240.6 %
Air Aging: 240 hours @ 100°C; 30 mil slabs; UL 1581
300 %
300 %
ASTM D-638
100% Modulus 0.0153 GPa
2.22 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -15.0 °C
5.00 °F
ASTM D-746
Oxygen Index 35 %
35 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F