Material Notes:
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D-785
Hardness, Shore D 78
78
ASTM D-2240
Tensile Strength, Yield 41.5 MPa
6020 psi
ASTM D-638
Tensile Modulus 2.91 GPa
422 ksi
ASTM D-638
Flexural Strength 71.77 MPa
10410 psi
ASTM D-790
Flexural Modulus 2.68 GPa
389 ksi
ASTM D-790
Izod Impact, Notched 8.65 J/cm

@Thickness 3.17 mm
16.2 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Gardner Impact 0.678 J
0.500 ft-lb
per mil, Method B, C-125 Tup; ASTM D-4226
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 61.78 °C
143.2 °F
unannealed; ASTM D-648