Axiall 36631 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 36631 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semi-rigid, 80°C rated riser insulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 - 1.38 g/cc
1.34 - 1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 52 - 58
52 - 58
delayed; ASTM D-2240
63 - 69
63 - 69
ASTM D-2240
Tensile Strength, Yield 23.2 MPa
3370 psi
ASTM D-638
Elongation at Yield 255 %
255 %
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Oxygen Index 31 %
31 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F