Axiall 3802 Vinyl Foam, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 3802 Vinyl Foam, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 0.600 - 0.700 g/cc
0.600 - 0.700 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 57.8
57.8
ASTM D-2240
Tensile Strength, Yield 13.2 MPa
1910 psi
ASTM D-638
Tensile Modulus 1.81 GPa
262 ksi
ASTM D-638
Flexural Strength 24.5 MPa
3550 psi
ASTM D-790
Flexural Modulus 1.03 GPa
149 ksi
ASTM D-790
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 12.8 kJ/m²
6.10 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 104 µm/m-°C

@Temperature 20.0 °C
58.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D-648
Processing Properties Metric English Comments
Zone 1 166 °C
330 °F
Zone 2 166 °C
330 °F
Zone 3 177 °C
350 °F
Zone 4 182 °C
360 °F
Die Temperature 185 °C
365 °F