Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 7020 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 7020 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityFlame RetardanceChemical ResistanceDurabilityColorabilityInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D-785
Hardness, Shore D 79
79
ASTM D-2240
Tensile Strength, Yield 45.5 MPa
6600 psi
ASTM D-638
Tensile Modulus 3.03 GPa
440 ksi
ASTM D-638
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Flexural Modulus 3.03 GPa
440 ksi
ASTM D-790
Izod Impact, Notched 9.61 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
18.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 147 kJ/m²
70.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 70.2 µm/m-°C

@Temperature 20.0 °C
39.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Cell Classification 14354
ASTM D-1784