Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Nilit Polynil® P50 Standard Viscosity Nylon 66 Description: Standard viscosityApplication: CompoundingInformation provided by NILIT. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Nilit Polynil® P50L Externally Lubricated Nylon 66 Description: Polynil P50L is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips. It is also suited for monofilament extrusion.Key characteristics: Ex.. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Quadrant EPP Duratron® PAI T4501 Polyamide-imide, compression molded bearing grade (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Fiberfil® J-60/10/E8 Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Total PSC 523 Polystyrene Polystyrene 523 is a high flow, high heat crystal. Specially designed for foam applications it has a very narrow molecular weight distribution. Performance in extruded loose fill foam is excellent d.. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Total PSC 524B Polystyrene Polystyrene 524B is a general purpose crystal polystyrene targeted for gloss coextrusion cap applications. It is specially formulated to reduce die buildup and die lines.Information provided by Tota.. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Total PSC 525 Polystyrene Polystyrene 525 is a crystal polystyrene for both injection molding and cap layer co-extrusion. Injection molding applications such as medical and laboratory parts, tumblers and jewel boxes demonstr.. |
|||
Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D-638 |
Axiall 7020 Rigid PVC, Extrusion Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF.. |