Material Notes:
Georgia Gulf 8240 is a general-purpose rigid PVC extrusion compound designed for applications requiring the following properties: Rigidity/StiffnessGlossImpact Strength & ToughnessFlame RetardantChemical ResistantThermoformabilityColorabilityInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 45.5 MPa
6600 psi
ASTM D-638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D-638
Flexural Strength 82.7 MPa
12000 psi
ASTM D-790
Flexural Modulus 3.34 GPa
485 ksi
ASTM D-790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D-256
Tensile Impact Strength 185 kJ/m²
88.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C
155 °F
ASTM D-648
Flammability, UL94 V-0
V-0
At 0.030 inch
Descriptive Properties Value Comments
Cell Classification 15363
ASTM D-1784
Users viewing this material also viewed the following: