Axiall 8740 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8740 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.41 g/cc
1.37 - 1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 71 - 77
71 - 77
delayed; ASTM D-2240
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Elongation at Yield 360 %
360 %
ASTM D-638
100% Modulus 0.00500 GPa
0.725 ksi
ASTM D-638
Tear Strength 28.0 kN/m
160 pli
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F