Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D412
Precision Polymer Engineering V75B Fluoroelastomer Compound
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B37, B38, EF31, EO78, F14, Z1, where Z1 = compressi..
Tensile Strength, Yield 12.1 MPa
1750 psi
chs 20 in/min; ASTM D412
Network Polymers Softflex® 6500
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tensile Strength, Yield 12.1 MPa
1750 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 12.1 MPa
1750 psi
Elastic; ASTM D412
Multibase Multi-Flex® TEA 4001-65 TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Tensile Strength, Yield >= 12.1 MPa
>= 1750 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7130 Fluorocarbon-Elastomer
FKM specially for oil & gas service.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D412
Teknor Apex APEX® 1700-70 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met..
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D412
Teknor Apex APEX® 90-A41R-65-NT Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by..
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D412
Vicone High Performance Rubber VicoSeal™ 106C-BK High Performance EPDM Rubber
Information provided by Vicone
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 53080A Moldings & Extrusions Flexible PVC
General purpose molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 8740 Moldings & Extrusions Flexible PVC
General purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio..
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 8743 Moldings & Extrusions Flexible PVC
A high quality extrusion compound recommended for weatherstrips, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 8747 Moldings & Extrusions Flexible PVC
Economical general purpose molding and extrusion compound with good flex whitening resistance especially in darker colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation i..
Tensile Strength, Yield 12.1 MPa
1750 psi
2 in/min (50 mm/min); ASTM D638
Bapolene® 2272 Polyethylene, Injection Grade
Bapolene LL2272 is a high flow, narrow molecular weight distribution, linear low density polyethylene injection resin. This resin offers excellent stress cracking resistance, flex life, low tempera..
Tensile Strength, Yield 12.1 MPa
1750 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 46234B Flexible PVC
Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.