Axiall 8778 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8778 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose compound recommended for extrusion and molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.51 - 1.55 g/cc
1.51 - 1.55 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 74 - 80
74 - 80
delayed; ASTM D-2240
Tensile Strength, Yield 9.549 MPa
1385 psi
ASTM D-638
Elongation at Yield 305 %
305 %
ASTM D-638
100% Modulus 0.00555 GPa
0.805 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Users viewing this material also viewed the following: