Material Notes:
Non-lead stabilized, flame retardant, non-migratory, 105°C insulation compound recommended for use in non-migratory applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.39 - 1.43 g/cc
1.39 - 1.43 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88
82 - 88
delayed; ASTM D-2240
Tensile Strength, Yield 15.9 MPa
2300 psi
ASTM D-638
Elongation at Yield 285.7 %
285.7 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
325 %
325 %
ASTM D-638
100% Modulus 0.009825 GPa
1.425 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Oxygen Index 27 %
27 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F