Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Azdel
Trade Name Plus
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AZDEL® C327-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural thin wall applications and where good glass distributions into features such as ribs and bosses is desired.Mechanical properties and mold shrinkage measured on flat plaques.Information provided by Azdel.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Laminate; ISO 1183
1.15 g/cc
1.15 g/cc
Molded; ISO 1183
Filler Content 31 %
31 %
By weight (ashing); Internal
Thickness 4320 microns
170 mil
Sheet; Internal
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
Measured on flat plaques; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527
Elongation at Break 2.8 %
2.8 %
ISO 527
Tensile Modulus 4.528 GPa
656.7 ksi
ISO 527
Flexural Strength 97.7 MPa
14200 psi
ISO 178
Flexural Modulus 4.26 GPa
618 ksi
ISO 178
Poissons Ratio 0.428
0.428
ISO 527
Izod Impact, Notched (ISO) 27.9 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
13.3 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Impact 2629

@Thickness 102 mm
2629

@Thickness 4.00 in
Multi-axial in Newtons, at max. load; ASTM D3763
Impact Test 12.1 J

@Thickness 102 mm
8.92 ft-lb

@Thickness 4.00 in
Multi-axial, at max. load; ASTM D3763
21.4 J

@Thickness 102 mm
15.8 ft-lb

@Thickness 4.00 in
Multi-axial, at failure; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 51.2 µm/m-°C

@Temperature -40.0 - 120 °C
28.4 µin/in-°F

@Temperature -40.0 - 248 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75
Descriptive Properties Value Comments
Color Black
Internal
Users viewing this material also viewed the following: