Polymer Property : CTE, linear = 51.2 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 51.2 µm/m-°C

@Temperature -40.0 - 120 °C
28.4 µin/in-°F

@Temperature -40.0 - 248 °F
ASTM E831
Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C327-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope..