BASF Caprolactam Tablets

Category Other Engineering Material
Manufacturer BASF
Trade Name Caprolactam Tablets
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Caprolactam Tablets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.500 - 0.550 g/cc
0.0181 - 0.0199 lb/in³
Density 1.105 g/cc
0.03992 lb/in³
pH 7.0 - 8.5
7.0 - 8.5
333 g/l
Viscosity Measurement 8.52

@Temperature 80.0 °C
8.52

@Temperature 176 °F
[mPa.s] Dynamic
Molecular Weight 113.16 g/mol
113.16 g/mol
Vapor Pressure 0.00000130 bar

@Temperature 20.0 °C
0.000975 torr

@Temperature 68.0 °F
0.0000890 bar

@Temperature 60.0 °C
0.0668 torr

@Temperature 140 °F
Thermal Properties Metric English Comments
Melting Point 69.3 °C
157 °F
Boiling Point 270.8 °C

@Pressure 0.1031 MPa
519.4 °F

@Pressure 14.96 psi
Flash Point >= 152 °C
>= 306 °F
DIN 51758
Descriptive Properties Value Comments
Color White
Commercial Status Europe
Ignition Temperature 365°C
DIN 51794
Solubility in Water 866.89