Material Notes:
Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also available in heat stabilized (Capron GR20 HS) and/or pigmented versions.Capron GR20 is ideally suited for more demanding performance applications such as safety helmet parts, washers, gears, engine and motor parts, chutes, and higher temperature environments.Data provided by Allied Signal.Processing: Max. water content 0.12%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.Melt Temperature: 270-295 degC (518-563 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate. Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
(Dry)
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM Data MD (Dry)
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ISO Data (Dry)
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ASTM data at 5 mm/min.
92.0 MPa
13300 psi
ISO value at 5mm/min.
Tensile Modulus 3.53 GPa
512 ksi
same value from ASTM and ISO test.
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Processing Properties Metric English Comments
Processing Temperature 275 °C
527 °F
See Materials Notes
Mold Temperature 95.0 °C
203 °F
See Materials Notes
Drying Temperature 85.0 °C
185 °F
See Materials Notes