Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | |
Plastcom SLOVAMID 6 FRC 1 PA6 with flame retardant Features: Determined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material p.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 3.17 mm |
0.011 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 0615 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® SK612SF NC010 PBT
(Unverified Data**) Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
DuPont Performance Polymers Crastin® SK615SF BK591 PBT
(Unverified Data**) Crastin® SK615SF BK591 is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast .. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided .. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
DSM Akulon® K223-KM6 Nylon 6-30% Mineral Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
Mold Temp 80°C; Melt Temp 300°C; 600 bar; ISO 294-4 |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | |
LATI Latilub 66-10T G/10 PA66, 10% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA High flow PPO+PA. Power distribution box applications. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm @Thickness 3.20 mm |
0.011 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ASTM D955 |
Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Linear Mold Shrinkage, Transverse | 0.011 - 0.014 cm/cm | 0.011 - 0.014 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF1758-BK2 33% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Sim. To ISO 294-4 |
DSM Arnite® TV4 461 KL (PBT+PET)-GF30 30% Glass Reinforced, Heat Stabilized, UV Stabilized, Excellent Surface Properties |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Sim. To ISO 294-4 |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
DSM Novamid® 1010GN2-15Z BK701 PA6-GF15 FR(17) 15% Glass Reinforced, Flame Retardant, Easy Molding Grade, Injection Molding, High Flow |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® HT XE 3996 PA*-GF30 Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designatio.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecomid® NA40 GR25 GR003 XA70 PA6.6, 25% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035 Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Eurotec® Tecomid® NB30 BK EF PA6, unfilled, black, suitable for electrostatic powder coating Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 3.20 mm |
0.011 in/in @Thickness 0.126 in |
DAM; ASTM D149 |
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | |
Eurotec® Tecodur® PB70 GR15 NL PBT 15% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.011 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture) Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Time 86400 sec |
0.011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RVN17SXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RVN17SXS is a compound based on PA 66 resin containing Long Glass Fiber, MoS2. Added features include; Wear Resistant. |